The stainless Tz series slag agglomerator is non-toxic and odorless, free of harmful components. It's suitable for slag removal in iron water and does not produce dust or pollute the environment. It has high dispersion, good slag agglomeration performance, fast bonding speed, good film-forming properties, and quick slag removal.
1. Iron ladle: After filling the molten iron ladle with molten iron, take an appropriate amount of this product and sprinkle it on the surface to quickly adhere the floating slag on the surface of the molten iron. Use a slag removal plate to remove the floating slag in one go.
2. Fan shaped ladle: When the fan-shaped ladle is filled with molten iron, sprinkle an appropriate amount of product on the surface, quickly remove it with an iron rake, and then evenly sprinkle an appropriate amount of product on the surface to form a protective film before pouring.
3. When the iron water in the induction furnace is heated to the slag removal temperature, take an appropriate amount of this product and sprinkle it into the furnace. Then, use a garbage stick or iron rod to remove it. The product can remove the slag and oxide on the surface of the iron.
The stainless Tz series slag agglomerator is non-toxic and odorless, free of harmful components. It's suitable for slag removal in iron water and does not produce dust or pollute the environment. It has high dispersion, good slag agglomeration performance, fast bonding speed, good film-forming properties, and quick slag removal.
This product uses an adsorption mechanism based on cohesive bonding. It has a high heat-resistant degree, does not melt itself, and does not produce secondary slag. The film formed on the iron water surface not only adsorbs and blocks molten slag but also has excellent insulation properties, effectively preventing iron water oxidation.
It's used for covering and insulating sand mold risers in steel castings and investment casting risers. Its appearance is a reddish-brown powder, non-toxic and odorless, with no harmful components.
Main Chemical Composition |
|||||
SiO2 |
AI2O3 |
Fe2O3 |
Na2O |
CaO |
K2O |
≥68 |
≥10 |
≥0.6 |
≥2.5 |
≥0.3 |
≥2.5 |
Physical Properties |
|||
Density g/cm3 |
Expansion Temperature℃ |
Expansion Multiplier |
Moisture Content% |
≥1.2 |
1300-1400 |
>5.0 |
≤0.4 |
Applicable to gray cast iron, ductile cast iron, and malleable cast iron, appearing...
Sand mold sprue of cast steel and cast iron, sprue of molten mold casting, appearance...
Plastic is an amorphous refractory material used in hot metal ladle.
A specialized, advanced refractory material designed specifically for foundry enterprises' steel...